SAE AMS5841E

SAE AMS5841E Cobalt-Nickel Alloy, Corrosion and Heat Resistant, Bars 19Cr 36Co 25Ni 7.0Mo 0.50Cb (Nb) 2.9Ti 0.20Al 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated For Work Strengthening

standard by SAE International, 08/01/2006

More details

Download

PDF AVAILABLE FORMATS IMMEDIATE DOWNLOAD
$34.32

$78.00

(price reduced by 56 %)

Full Description

This specification covers a high strength, corrosion and heat resistant cobalt-chromium-nickel alloy in the form of bars.

These bars have been used typically for applications requiring a combination of high strength up to 1100 degrees F (593 degrees C), good tension-tension fatigue strength, toughness, and ductility, but usage is not limited to such applications. This alloy exhibits exceptionally good resistance to corrosion, crevice-corrosion, stress-corrosion cracking, and elevated temperature relaxation.