SAE AMS5841F Cobalt-Nickel Alloy, Corrosion and Heat-Resistant, Bars, 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe, Vacuum Induction Plus Vacuum Consumable Electrode Melted, Solution Heat Treated for Work Strengthening

standard by SAE International, 09/13/2011

More details

Download

PDF AVAILABLE FORMATS IMMEDIATE DOWNLOAD
$32.76

$78.00

(price reduced by 58 %)

Full Description

This specification covers a high strength, corrosion and heat resistant cobalt-chromium-nickel alloy in the form of bars.

These bars have been used typically for applications requiring a combination of high strength up to 1100 mDF (593 mDC), good tension-tension fatigue strength, toughness, and ductility, but usage is not limited to such applications. This alloy exhibits exceptionally good resistance to corrosion, crevice-corrosion, stress-corrosion cracking, and elevated temperature relaxation.